The first breakdown attempt was to ball mill the larger parts (~0.98 x 1.96 x 0.39 in [~25 mm x 50 mm x 10 mm]) directly. This was unsuccessful. So, in all subsequent breakdown processes the spent ceramic was reduced by manually hammering until the largest size was approximately 0.3 in. (8 mm). Then they were tumble-ball milled for five hours.